It is the process of determining the Z qualities of the materials according to the percentage reduction ratio of the rupture area by removing the sample perpendicular to the product surface (in the direction of thickness) and pulling it with the help of a tensile tester until it breaks.
In our laboratory, the mentioned test is carried out with the INSTRON 600 kN Universal Tensile-Pressing device.